My Infoweb
English
Editorial team · Hydraulics, Pneumatics

PLASMATREAT TEST INKS

PLASMATREAT TEST INKS
A simple and effective method for evaluating the control and measurement results obtained with PLASMATREAT test inks before treating material surfaces such as plastic, metal or glass for printing, bonding or painting...

PLASMATREAT test inks for analyzing, measuring and determining the surface tension of a surface to be treated.

A simple and effective method for evaluating the control and measurement results obtained with PLASMATREAT test inks before treating material surfaces such as plastic, metal or glass for printing, bonding or painting.

PLASMATREAT TEST INKS
Whatever the material used (plastic, metal, glass, ...), the surface to be treated depends specifically on a suitable surface tension, and the same applies to any liquid substance (ink, adhesive, paint, ...) that may be used, which has its own surface tension.

To optimize adhesion with these liquid substances, and to ensure that it lasts without strain and performs particularly well, the surface tension of the material used must be higher than that of the liquid. Thus, thanks to a PLASMATREAT treatment applied with the OPENAIR® plasma system, a significant increase in surface tension is obtained, which promotes and improves the printing, bonding or painting of any surface with optimal durability.

USING PLASMATREAT TEST INKS
To assess the wetting quality of a surface to be treated, the test ink is applied to the surface with a small brush integrated into the cap of the bottle. After the test ink has been applied, if the edges of the ink line remain stable for a few seconds, this indicates good wetting of the surface, and the tension of the substrate is at least equal to the value of the test ink.

On the other hand, if the edges of the applied test ink retract, this means the test must be continued by applying an ink of the next lower value. Thus, by successively using different grades of test ink, it is entirely possible to get close to the exact surface tension value of the material to be analyzed.

The surface tension of the test ink with which the surface is no longer wetted corresponds to the tension being sought. The test ink with the next higher surface tension no longer wets the surface. Finally, test inks must never be mixed with one another, in order to avoid any misinterpretation of the test.